鹽城環氧自流平地坪底漆層的涂布是無錫環氧自流平地坪施工過程中最基礎的一步。底漆層處于環氧地坪基面與環氧地坪涂層之間,這樣可以增強環氧地坪涂層與地面的附著力。環氧地坪漆廠家根據多年施工經驗來談談有關環氧地坪漆底漆用量與使用注意事項,環氧地坪底漆的使用量受外部影響表現在如下幾個方面:影響環氧環氧地坪漆底漆用量的因素: The coating of epoxy floor paint primer is the most basic step in the construction of epoxy floor paint. The primer layer is between the base of the floor and the epoxy floor coating, which can enhance the adhesion between the epoxy floor coating and the ground. According to years of construction experience, Guanglei floor paint manufacturer talks about the amount of epoxy floor paint primer and the matters needing attention. The use of epoxy floor primer is affected by external factors as follows: factors affecting the amount of epoxy floor paint primer: 影響無錫環氧自流平地坪底漆使用量的最主要因素是地坪施工基面的粘結強度進而影響整體的強度。施工無錫環氧自流平地坪漆一般要求混凝土地面的強度大于C25,較好的地面底漆用量一般在0.15~0.2kg/m2,若地面強度過低,地面疏松,易起砂,則無錫環氧自流平地坪底漆的使用量則會根據實際環境跟情況而改變用量。
The most important factor affecting the use of epoxy floor primer is the bond strength of the construction base and then the overall strength. Construction of epoxy floor paint generally requires that the strength of concrete floor is greater than C25, and the amount of better floor primer is generally 0.15-0.2 kg/m2. If the floor strength is too low, the ground is loose and easy to sand, the use of epoxy floor primer will change according to the actual environment and the situation.
此外,如果地坪施工基面強度低,但又沒有涂布適當適量的無錫環氧自流平地坪底漆來增加地坪基面粘結強度,則無錫環氧自流平地坪質量較差。如果地坪上有叉車等重物時,無錫環氧自流平地坪就可能會連同無錫環氧自流平地坪基面一起被壓陷拉裂。
In addition, the quality of the epoxy flooring is poor if the strength of the flooring construction base is low, but the proper amount of epoxy flooring primer is not coated to increase the cohesive strength of the flooring base. If there are forklift trucks and other weights on the floor, the epoxy floor may be collapsed and cracked together with the epoxy floor base.
因此,在無錫環氧自流平地坪施工時,一定要保證底漆的涂布量適量。如果地面整體強度過低,則可根據承重及強度要求選用環氧砂漿涂層,或者有條件的可重新進行地面改造,詳情可咨詢光磊地坪漆廠家技術部,這樣可以減少不必要得成本損耗。
Therefore, in the construction of epoxy floor, it is necessary to ensure the proper amount of primer coating. If the overall strength of the ground is too low, epoxy mortar coating can be selected according to the load-bearing and strength requirements, or the ground can be reconstructed if conditions permit. Details can be consulted with the technical department of Guanglei floor paint manufacturer, so as to reduce unnecessary cost losses.
無錫環氧自流平地坪底漆施工注意事項:
Points for attention in the construction of epoxy floor paint primer:
用刷涂、輥涂或噴涂的方法施工封閉地坪漆底漆一道至兩道,兩道之間的間隔時間在8h以上,但不能大于48h。對于舊地面,應增加一道底漆。底漆施工時應注意涂布均勻,涂膜無明顯的厚度差異,防止漏涂。用輥涂法施工應注意余料堆積情況。底漆封閉不完全(漏涂)時,會發生附著不牢、涂膜起泡等現象。
Brush, roll or spray method is used to construct one or two primers for closed floor paint. The interval between the two primers is more than 8 hours, but not more than 48 hours. For the old ground, a primer should be added. During primer construction, attention should be paid to uniform coating, no obvious thickness difference of coating film, to prevent leakage of coating. Pay attention to the accumulation of surplus materials in roller coating construction. When the primer is incompletely sealed (missing coating), there will be some phenomena such as weak adhesion and blistering of the coating film.
1.底漆漆膜厚度根據底漆品種確定,應注意控制。表面無浮塵及松散砂粒。
1. The thickness of primer film is determined according to the type of primer. Attention should be paid to its control. There is no floating dust and loose sand on the surface.
2.含顏填料的底漆在使用前和使用過程應注意攪拌均勻。
2. The primer containing pigments and fillers should be stirred evenly before use and during use.
3.注意遵守干燥的規范。在底涂上如涂含有強溶劑的涂料時,底漆必須干透,以免出現咬底等漆病。
3. Pay attention to the standard of drying. When the primer is coated with paint containing strong solvents, the primer must be thoroughly dried to avoid primer biting and other paint diseases.
4.增加下一道涂層與底漆間的附力,可在涂布前將底漆打磨。
4. To increase the adhesion between the next coating and the primer, the primer can be polished before coating.
5.要在漆前表面處理以后嚴格按照規定的時間及時涂布底漆。還要根據底漆品種規定的條件在底漆干燥后規定時間范圍內涂下一道漆。過早涂布可能引起咬底及底漆中溶劑揮發困難導致漆膜干燥時間延長、固化不良的情況;涂布過遲可能引起層間附著不良,且過遲涂布易由于粉塵積累或其他污染影響表觀。
5. Primer should be coated in time after surface treatment. Also, according to the conditions specified by the primer varieties, a coat should be applied within the prescribed time range after the primer is dried. Early coating may lead to underbiting and difficulty in volatilization of solvents in primers, which may lead to prolonged drying time and poor curing of the film; late coating may lead to poor adhesion between layers, and late coating may easily affect the appearance due to dust accumulation or other pollution.